Application: | Aviation, Industrial |
---|---|
Standard: | GB, ASTM |
Purity: | 85%-97% |
Grade |
State |
Density (g/cc) |
UST |
Elongation (%) |
Hardness (HRC) |
Impact toughness (MJ/m2) |
W273 |
|
17.10±0.15 |
≥900 |
≥24 |
≥23 |
≥1.3 |
Heat treatment |
||||||
W263 |
|
17.25±0.15 |
≥900 |
≥23 |
≥23 |
≥1.2 |
Heat treatment |
||||||
W262 |
|
17.50±0.15 |
≥910 |
≥25 |
≥24 |
≥1.1 |
Heat treatment |
||||||
W261 |
|
17.60±0.15 |
≥920 |
≥24 |
≥24 |
≥1 |
Heat treatment |
||||||
W253 |
|
17.40±0.15 |
≥900 |
≥22 |
≥24 |
≥1.1 |
Heat treatment |
||||||
W252 |
|
17.65±0.15 |
≥920 |
≥18 |
≥24 |
≥0.6 |
Heat treatment |
||||||
W243 |
|
17.60±0.15 |
≥920 |
≥20 |
≥24 |
≥0.9 |
Heat treatment |
||||||
W242 |
|
18.10±0.10 |
≥833 |
≥3 |
≥25 |
≥0.1 |
Heat treatment |
||||||
W242A |
|
17.90±0.10 |
≥910 |
≥10 |
≥25 |
≥0.45 |
Heat treatment |
||||||
W232 |
|
18.10±0.15 |
≥920 |
≥14 |
≥25 |
≥0.45 |
Heat treatment |
||||||
W231 |
|
18.30±0.15 |
≥920 |
≥12 |
≥26 |
≥0.3 |
Heat treatment |
||||||
W221 |
|
18.50±0.15 |
≥920 |
≥10 |
≥27 |
≥0.22 |
Heat treatment |
||||||
W173 |
|
17.20±0.15 |
≥600 |
≥2 |
≥26 |
- |
Heat treatment |
||||||
W125 |
|
17.65±0.15 |
≥600 |
≥2 |
≥27 |
- |
Heat treatment |
||||||
W131 |
|
18.15±0.15 |
≥600 |
≥1 |
≥28 |
- |